Questions on using Hood's QDPF
-
- Posts: 5951
- Joined: Tue Dec 13, 2011 7:44 pm
Re: Questions on using Hood's QDPF
I might also throw in that zinsser seal-coat, mixed 50/50 with mineral spirits, can be wiped on, left for a couple of hours, then rubbed off with 0000 steel wool, and gives a completely clear pore fill that works fine with topcoats. It will shrink a little so I use a second coat. .02
-Under permanent construction
Re: Questions on using Hood's QDPF
Hi Bob, Sorry to hear that your having some problems with Hood's Grain filler. I also used Hood's filler on the two guitars that I have finished, and had the same problems that you mentioned, brush marks and drying to fast. I applied two coats on the 1st guitar and 3 coats on the 2nd, with the 2nd guitar turning out better, but not great. I talked with Eric the owner of Hood Products, He suggested that I use his Magna Shield Retarder, which slows down the drying time. He said to mix 5% of the retarder by volumn, with the QDPF. I haven't decided on what filler I'm going to use on the present project.
Eric also said that foam brushes could NOT be use when applying QDPF.
Charlie
Eric also said that foam brushes could NOT be use when applying QDPF.
Charlie